EFFECT OF MICROSTRUCTURE AND RELATIVE HUMIDITY ON ATMOSPHERIC PITTING CORROSION OF DUPLEX STAINLESS STEEL BENEATH MGCL2 DROPS

Authors

  • Safa A. Ali Department of Physics, Faculty of Science, University of Zakho, Zakho,Kurdistan Region-Iraq
  • Haval B. Mohammed Ali Department of Physics, Faculty of Science, University of Zakho

DOI:

https://doi.org/10.25271/sjuoz.2023.11.2.1047

Keywords:

Microstructure, Relative Humidity, Atmospheric Pitting Corrosion, Duplex Stainless Steel

Abstract

One of the main issues for intermediate-level nuclear waste (ILW) is atmospheric corrosion in stainless steel. The impact of microstructure on the pit shapes on three orientations of the duplex stainless steel DSS 2205 plate and the relative humidity impact on the atmospheric corrosion pits of DSS beneath MgCl2 drops is determined through the use of four characterization tools: X-ray diffraction (XRD), Energy dispersive X-ray (EDX) analyses, Scanning electron microscopy (SEM), and optical microscopy. The pits on the top surface (LT) appears layered like an attack and mostly hemispherical, while the long transverse (LS) and short transverse (ST) planes reveal elongated strings. The map scan of EDX indicates mixed oxide inclusions and MnS inclusion existing in the steel alloy and the XRD analyses present the existence of two-phase both austenite γ and ferrite α peaks. The pit shape and area were influenced by relative humidity (RH) change. At RH 35% the trend of pits in 1-week exposure revealed a larger area of pit mouth than in RH 45%. For the same exposure time and in both RHs, the area seemed to be greater at the droplet’s center than in the edge of the droplet.

References

ASTM, E. (1985) (1985) ‘Standard practice for maintaining constant relative humidity by means of aqueous solutions’, pp. 790–795.

Cvijović, Z. and Radenković, G. (2006) ‘Microstructure and pitting corrosion resistance of annealed duplex stainless steel’, Corrosion Science, 48(12), pp. 3887–3906. doi: 10.1016/j.corsci.2006.04.003.

Deng, B. et al. (2009) ‘Evaluation of localized corrosion in duplex stainless steel aged at 850 °C with critical pitting temperature measurement’, Electrochimica Acta, 54(10), pp. 2790–2794. doi: 10.1016/j.electacta.2008.11.038.

Devaraj, A. (2022) ‘Directly Monitoring the Shift in Corrosion Mechanisms of a Model FeCrNi Alloy Driven by Electrical Potential’, pp. 1–16.

Ghahari, M. et al. (2015) ‘Synchrotron X-ray radiography studies of pitting corrosion of stainless steel: Extraction of pit propagation parameters’, Corrosion Science, 100, pp. 23–35. doi: 10.1016/j.corsci.2015.06.023.

Haval Bashar MohammedAli (2016) Atmospheric Pitting Corrosion of Stainless Steel. University of Birmingham.

Laya-Guo (2019) ‘The effect of relative humidity change on atmospheric pitting corrosion of stainless steel 304L’, Corrosion Science, 150, pp. doi: 10.1016/j.corsci.2019.01.033.

Lei, Z. et al. (2021) ‘Effect of microstructure distribution on pitting initiation and propagation of 2002 duplex stainless steel’, Journal of the Chinese Society of Corrosion and Protection, 41(6), pp. 837–842. doi: 10.11902/1005.4537.2020.183.

Li, J. et al. (2022) ‘Study on Pitting Corrosion Behavior and Semi in-situ Pitting Corrosion Growth Model of 304L SS With Elastic Stress in NaCl Corrosion Environment’, Corrosion Science, p. 110862.

Lo, I. H. and Tsai, W. T. (2007) ‘Effect of selective dissolution on fatigue crack initiation in 2205 duplex stainless steel’, Corrosion Science, 49(4), pp. 1847–1861. doi: 10.1016/j.corsci.2006.10.013.

Maier, B. and Frankel, G. S. (2010) ‘Pitting Corrosion of Bare Stainless Steel 304 under Chloride Solution Droplets’, Journal of The Electrochemical Society, 157(10), p. C302. doi: 10.1149/1.3467850.

Mampuya, M. B. et al. (2021) ‘Effect of heat treatment on the microstructure of duplex stainless steel 2205’, Materials Today: Proceedings, 38(xxxx), pp. 1107–1112. doi: 10.1016/j.matpr.2020.06.196.

Mohammad-Ali (2016) Atmospheric Pitting corrosion of Stainless steel. University of Birmingham.

Mohammad-Ali (2018) ‘The efect of microstructure on the morphology of atmospheric corrosion pits of type 304L’, Corrosion. doi: 10.5006/2935.

Moreıra, É. P. et al. (2023) ‘Risk Analysis Related to the Corrosıon of Atmospheric Storage Tanks: A Multimethodological Approach Using the FRAM and the ELECTRE-MOr Methods’, in Pervasive Computing and Social Networking. Springer, pp. 245–257.

Van Nam, T., Tada, E. and Nishikata, A. (2015) ‘Pit initiation and repassivation of stainless steels exposed to cyclic relative humidity changes’, Journal of the Electrochemical Society, 162(9), p. C419.

Örnek, C. (2015) ‘Performance Characterisation of Duplex Stainless Steel in Nuclear Waste Storage Environment’, Thesis, pp. 95–110.

Örnek, C. and Engelberg, D. L. (2015) ‘SKPFM measured Volta potential correlated with strain localisation in microstructure to understand corrosion susceptibility of cold-rolled grade 2205 duplex stainless steel’, Corrosion Science, 99, pp. 164–171. doi: 10.1016/j.corsci.2015.06.035.

Park, J. H. and Kang, Y. (2017) ‘Inclusions in Stainless Steels − A Review’, Steel Research International, 88(12), pp. 1–26. doi: 10.1002/srin.201700130.

Potgieter, J. H. et al. (1996) ‘Corrosion behaviour of duplex stainless steels containing minor ruthenium additions in reducing acid media’, Journal of Applied Electrochemistry, 26(11), pp. 1103–1110. doi: 10.1007/BF00243734.

Potgieter, J. H. et al. (2008) ‘Influence of nickel additions on the corrosion behaviour of low nitrogen 22% Cr series duplex stainless steels’, Corrosion Science, 50(9), pp. 2572–2579. doi: 10.1016/j.corsci.2008.05.023.

Pramanik, S., Bera, S. and Ghosh, S. K. (2014) ‘Influence of cold rolling on microstructural evolution in 2205 duplex stainless steel’, Steel Research International, 85(5), pp. 776–783. doi: 10.1002/srin.201300293.

Rodrigues, D. G. et al. (2019) ‘Effect of low cold-rolling strain on microstructure, texture, phase transformation, and mechanical properties of 2304 lean duplex stainless steel’, Materials Characterization, 150(February), pp. 138–149. doi: 10.1016/j.matchar.2019.02.011.

Sheik, S. et al. (2022) ‘Effect of microstructural morphology on corrosion susceptibility of austenitic and super austenitic stainless steels’, Materials Today: Proceedings, 66, pp. 514–518.

Stewart, J. and Williams, D. E. (1992) ‘The initiation of pitting corrosion on austenitic stainless steel: on the role and importance of sulphide inclusions’, Corrosion Science, 33(3). doi: 10.1016/0010-938X(92)90074-D.

Street, S. R. et al. (2015) ‘Atmospheric pitting corrosion of 304L stainless steel: The role of highly concentrated chloride solutions’, Faraday Discussions, 180, pp. 251–265. doi: 10.1039/c4fd00246f.

Street, S. R. et al. (2018) ‘The effect of deposition conditions on atmospheric pitting corrosion location under Evans droplets on type 304L stainless steel’, Corrosion, 74(5), pp. 520–529. doi: 10.5006/2614.

Tan, H. et al. (2011) ‘Annealing temperature effect on the pitting corrosion resistance of plasma arc welded joints of duplex stainless steel UNS S32304 in 1.0M NaCl’, Corrosion Science, 53(6), pp. 2191–2200. doi: 10.1016/j.corsci.2011.02.041.

Tsutsumi, Y., Nishikata, A. and Tsuru, T. (2005) ‘Initial Stage of Pitting Corrosion of Type 304 Stainless Steel under Thin Electrolyte Layers Containing Chloride Ions’, Journal of The Electrochemical Society, 152(9), p. B358. doi: 10.1149/1.1992470.

Tsutsumi, Y., Nishikata, A. and Tsuru, T. (2007) ‘Pitting corrosion mechanism of Type 304 stainless steel under a droplet of chloride solutions’, Corrosion Science, 49(3), pp. 1394–1407. doi: 10.1016/j.corsci.2006.08.016.

Wang, H. and Wang, T. (2021) ‘Influence of Hot Rolling and Solution Treatment on the Microstructure and Mechanical Properties of High-Boron Duplex Stainless Steel 0Cr21Ni5Ti-2B’, Metal Science and Heat Treatment, 63(3–4), pp. 126–131. doi: 10.1007/s11041-021-00658-w.

Weirich, T. D. et al. (2019) ‘Humidity Effects on Pitting of Ground Stainless Steel Exposed to Sea Salt Particles’, Journal of The Electrochemical Society, 166(11), pp. C3477–C3487. doi: 10.1149/2.0551911jes.

Wranglen, G. (1974) ‘Pitting and sulphide inclusions in steel’, Corrosion Science, 14(5), pp. 331–349. doi: 10.1016/S0010-938X(74)80047-8.

Yoon, B. J. and Ahn, Y. S. (2022) ‘Correction to: Effect of Aging on Pitting Corrosion Resistance of 21Cr Lean Duplex Stainless Steel with Different Molybdenum Contents (Journal of Materials Engineering and Performance, (2022), 10.1007/s11665-022-07478-w)’, Journal of Materials Engineering and Performance, p. 11665. doi: 10.1007/s11665-022-07588-5.

Zhang, Y. et al. (2020) ‘Investigation of micro-electrochemical activities of oxide inclusions and microphases in duplex stainless steel and the implication on pitting corrosion’, Materials and Corrosion, 71(6), pp. 876–886. doi: 10.1002/maco.201911335.

Zhu, Y. et al. (2020) ‘Quantification of the Atmospheric Corrosion of 304 and 2205 Stainless Steels Using Electrochemical Probes Based on Thevenin Electrochemical Equivalent Circuit Model’, Transactions of Tianjin University, 26(3), pp. 218–227. doi: 10.1007/s12209-020-00242-y.

Downloads

Published

2023-05-30

How to Cite

Ali, S. A., & Mohammed Ali, H. B. (2023). EFFECT OF MICROSTRUCTURE AND RELATIVE HUMIDITY ON ATMOSPHERIC PITTING CORROSION OF DUPLEX STAINLESS STEEL BENEATH MGCL2 DROPS. Science Journal of University of Zakho, 11(2), 244–253. https://doi.org/10.25271/sjuoz.2023.11.2.1047

Issue

Section

Science Journal of University of Zakho